Thermoelectric — Chemical structure modulation in conductive MOFs by adjusting the oxidation state of the ligand and introducing alkali metal ions

Measurement evidence

Thermoelectric

Chemical structure modulation in conductive MOFs by adjusting the oxidation state of the ligand and introducing alkali metal ions · Wu X., Wu H., Wu S. et al. · Chemical Communications · 2022 · 2702-2705

1 measurement group · 2 results

Reported values remain attached to the sample, method, conditions, extraction quality and source location that produced them.

Seebeck coefficient measurement

MnHHB compressed cuboid pellet · Pellet

MnHHB at 300 K; five trials shown in Fig. S11.

Temperature
300
Geometry
Pellet, geometry not otherwise specified
Context
pristine framework pellet
Measurement source
p. 9 · Supporting figures and tables · Figure S11
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
Power factor at 300 K3 x 10^-4 uW m^-1 K^-2Caption
Exact Reported
p. 9 · Supporting figures and tables · Figure S11
Average Seebeck coefficient at 300 K23.8 uV K^-1Caption
Exact Reported
p. 9 · Supporting figures and tables · Figure S11