Electrical Transport — Isoreticular Modulation of Electrical Conduction and Magnetic Properties in Semiconducting Lanthanide-based Based Metal−Organic Frameworks

Measurement evidence

Electrical Transport

Isoreticular Modulation of Electrical Conduction and Magnetic Properties in Semiconducting Lanthanide-based Based Metal−Organic Frameworks · Qing H., Diamond B.G., Chan J.Y.M. et al. · Angewandte Chemie - International Edition · 2026 · e8403106

4 measurement groups · 8 results

Reported values remain attached to the sample, method, conditions, extraction quality and source location that produced them.

four-probe DC conductivity on pelletised powder

Eu-HHTP powder · Powder

temperature_range: variable temperature; geometry: pelletised powder

Measurement source
5 · Electronic Structures and Electrical Conductivity
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
average activation energy from Arrhenius fit0.29 eV (+/- 0.04)+/- 0.04Text
Exact Reported
5 · Electronic Structures and Electrical Conductivity
average bulk electrical conductivity at 300 K3.0 (+/- 2.1) x 10^-3+/- 2.1 x 10^-3Text
Exact Reported
5 · Electronic Structures and Electrical Conductivity

four-probe DC conductivity on pelletised powder

Gd-HHTP powder · Powder

temperature_range: variable temperature; geometry: pelletised powder

Measurement source
5 · Electronic Structures and Electrical Conductivity
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
average activation energy from Arrhenius fit0.31 eV (+/- 0.02)+/- 0.02Text
Exact Reported
5 · Electronic Structures and Electrical Conductivity
average bulk electrical conductivity at 300 K7.6 (+/- 3.0) x 10^-4+/- 3.0 x 10^-4Text
Exact Reported
5 · Electronic Structures and Electrical Conductivity

four-probe DC conductivity on pelletised powder

Sm-HHTP powder · Powder

temperature_range: variable temperature; geometry: pelletised powder

Measurement source
5 · Electronic Structures and Electrical Conductivity
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
average activation energy from Arrhenius fit0.22 eV (+/- 0.02)+/- 0.02Text
Exact Reported
5 · Electronic Structures and Electrical Conductivity
average bulk electrical conductivity at 300 K4.3 (+/- 3.7) x 10^-3+/- 3.7 x 10^-3Text
Exact Reported
5 · Electronic Structures and Electrical Conductivity

four-probe DC conductivity on pelletised powder

Tb-HHTP powder · Powder

temperature_range: variable temperature; geometry: pelletised powder

Measurement source
5 · Electronic Structures and Electrical Conductivity
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
average activation energy from Arrhenius fit0.33 eV (+/- 0.03)+/- 0.03Text
Exact Reported
5 · Electronic Structures and Electrical Conductivity
average bulk electrical conductivity at 300 K2.7 (+/- 1.0) x 10^-4+/- 1.0 x 10^-4Text
Exact Reported
5 · Electronic Structures and Electrical Conductivity