Hall-effect measurement
Iodine-treated Co-BDC LBL film on amine-functionalised glass · Thin Film
HMS-300 ECOPIA Hall-effect instrument at 25 C after iodine treatment.
| Property | Reported value | Normalised value | Uncertainty | Origin and quality | Source |
|---|---|---|---|---|---|
| Co-BDC hole carrier concentration after iodine treatment | +1.14 x 10^11 cm^-3 | — | — | Text Exact Reported | p004 / article p.22672 · Results and discussion |
| Co-BDC hole mobility after iodine treatment | 21.2 cm^2 V^-1 s^-1 | — | — | Text Exact Reported | p004 / article p.22672 · Results and discussion |