Diffraction Structure — Dual single atomic Fe-Ni sites in N‑doped nanoporous carbon for high-efficiency potassium periodate activation toward pollutant abatement

Measurement evidence

Diffraction Structure

Dual single atomic Fe-Ni sites in N‑doped nanoporous carbon for high-efficiency potassium periodate activation toward pollutant abatement · Yao Y., Ma Z., Ma Z. et al. · Separation and Purification Technology · 2025 · 128091

2 measurement groups · 3 results

Reported values remain attached to the sample, method, conditions, extraction quality and source location that produced them.

X-ray diffraction (XRD)

Fe2Ni1-NC-900 · Powder

Carbonised FeNi-NC catalysts and controls; graphitic carbon peak and absence of metal crystals assessed.

Geometry
powder
Context
MOF-derived carbon catalysts
Measurement source
3-4 · 3.1 Characterizations of the synthesized catalysts · Figure 1b; Figure S1b-c
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
FeNi-NC graphitic carbon XRD peakbroad diffraction peak at about 23 degrees assigned to the (002) plane of graphitic carbonaboutText
Approximate
4 · 3.1 · Figure 1b
No metal crystal formationNo metal crystal was formed in the carbonaceous matrix; metals may be atomically dispersed.Qualitative
Qualitative
4 · 3.1 · Figure 1b

X-ray diffraction (XRD)

Fe&Ni-ZnO/ZIF-8 precursor · Powder

PANalytical X'pert diffractometer with Ni-filtered Cu Kalpha radiation at 40 kV/40 mA; precursor patterns compared with ZIF-8.

Geometry
powder
Context
ZIF-8-derived composite precursor
Measurement source
4 · 2.3; 3.1 · Figure S1a
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
ZIF-8-derived precursor diffraction assignmentFe-ZnO/ZIF-8, Ni-ZnO/ZIF-8, FeNi-ZnO/ZIF-8 and ZnO/ZIF-8 exhibit distinct diffraction peaks aligning with ZIF-8.Qualitative
Qualitative
4 · 3.1 · Figure S1a