temperature-dependent in-plane four-contact conductivity/resistivity
Ni-mba-K conductivity pellet · Pellet
Four-arm Lakeshore probe station under vacuum (1e-4 Pa); gold contacts; pellet thickness 20-40 um.
| Property | Reported value | Normalised value | Uncertainty | Origin and quality | Source |
|---|---|---|---|---|---|
| electrical conductivity at 120 deg C | about 1 x 10^-9 S cm-1 | — | — | Figure Axis Approximate | SI p.S2 · Figure S3 · Figure S3b |
| electrical conductivity at 30 deg C | >10^-11 S cm-1 | — | — | Text Range | main p.4 (journal p.17281) · 3.1. Structural Characterization · Figure S3b |
| electrical conductivity at 60 deg C | about 4 x 10^-11 S cm-1 | — | — | Figure Axis Approximate | SI p.S2 · Figure S3 · Figure S3b |
| electrical conductivity at 90 deg C | about 8 x 10^-11 S cm-1 | — | — | Figure Axis Approximate | SI p.S2 · Figure S3 · Figure S3b |