Partial recipeSource: Main
Route 1: Drop Cast
3 · Preparation of modified electrodes
SolventsDMF
Atmosphereair drying after electrode cleaning; dried under infrared light after drop-casting
Substrate orientationpolished glassy carbon electrode
Work-upGCE polished with 0.3 and 0.05 um alumina, rinsed with ethanol and deionised water in an ultrasonic bath, dried in air; CoPc-Cu MOF suspension dropped on GCE and dried under infrared light.
Show 2 structured reagent records
| Role | Reagent | Amount / concentration | Source |
|---|---|---|---|
| Other | CoPc-Cu MOF suspension | 3 ul reported in electrode preparation; 5 ul selected as optimum in optimisation · 3 mg ml-1 in DMF | 3 · Preparation of modified electrodes |
| Solvent | DMF | dispersion solvent | 3 · Preparation of modified electrodes |