Ex situ XRD during first charge-discharge cycle
Ni-CAT nanorod lithium-ion battery anode electrode · Electrode
XRD patterns during discharge to 1.0/0.5/0.01 V and charge to 1.5/3.0 V; used to infer structural change and recovery.
| Property | Reported value | Normalised value | Uncertainty | Origin and quality | Source |
|---|---|---|---|---|---|
| post-charge c-axis reflection | 2theta ~27.3 deg reflection cannot be observed after charge | — | — | Text Approximate | 3 · Results · Fig. S6 |
| XRD change on discharge | main peaks weakened and even disappear with discharging | — | — | Text Qualitative | 3 · Results · Fig. S6 |