Spectroscopy — Effective visible-light CO2 photoreduction over (metallo)porphyrin-based metal–organic frameworks to achieve useful hydrocarbons

Measurement evidence

Spectroscopy

Effective visible-light CO2 photoreduction over (metallo)porphyrin-based metal–organic frameworks to achieve useful hydrocarbons · Hariri R., Dehghanpour S. · Applied Organometallic Chemistry · 2021 · e6422

3 measurement groups · 5 results

Reported values remain attached to the sample, method, conditions, extraction quality and source location that produced them.

Fourier transform infrared spectroscopy (FT-IR)

PCN-222(Fe) · Powder

FT-IR spectra for PCN-222(Fe, Co, Ni and Cu) recorded on Bruker Tensor 27 using KBr pellets over 4000-400 cm-1; spectra in SI Figure S1.

Context
pristine metalloporphyrinic MOF series
Measurement source
3 · Characterization of catalyst · Figure S1
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
FT-IR COO stretching bands for PCN-222(Fe, Co, Ni, Cu)asymmetric COO: 1701, 1702, 1707, 1702 cm-1; symmetric COO: 1402, 1407, 1415, 1410 cm-1Text
Exact Reported
3 · Characterization of catalyst · Figure S1
FT-IR M-N bands for PCN-222(Fe, Co, Ni, Cu)M-N peaks: 999, 1011, 995, 1009 cm-1Text
Exact Reported
3 · Characterization of catalyst · Figure S1

Photoluminescence spectroscopy

PCN-222(Fe) · Powder

PL spectra recorded by Cary Eclipse fluorescence spectrophotometer; main Figure 5 uses 410 nm excitation for PCN-222(Fe), PCN-222(Co), PCN-222(Cu), PCN-222(Ni), and PCN-222(no metal).

Context
metalloporphyrinic MOF versus nonmetal PCN-222 control
Measurement source
4 · Characterization of catalyst · Figure 5
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
PL emission intensity trendPCN-222(M) emission band intensity is lower than nonmetal PCN-222Text
Qualitative
3-4 · Characterization of catalyst · Figure 5

UV-vis absorption spectroscopy

PCN-222(Fe) · Powder

UV-vis spectra of PCN-222(M) and metalloporphyrin precursors; spectra are in missing SI Figures S2-S3.

Context
pristine metalloporphyrinic MOF series
Measurement source
3 · Characterization of catalyst · Figure S3
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
PCN-222(M) visible-light absorption lower wavelength400 nm lower edge of reported strong absorption rangeText
Range
3 · Characterization of catalyst · Figure S3
PCN-222(M) visible-light absorption upper wavelength700 nm upper edge of reported strong absorption rangeText
Range
3 · Characterization of catalyst · Figure S3