Porosity — Proton-electron coupling and mixed conductivity in a hydrogen-bonded coordination polymer

Measurement evidence

Porosity

Proton-electron coupling and mixed conductivity in a hydrogen-bonded coordination polymer · Park M., Ju H., Oh J. et al. · Nature Communications · 2025 · 1316

2 measurement groups · 5 results

Reported values remain attached to the sample, method, conditions, extraction quality and source location that produced them.

BET N2 adsorption, Microtrac MRB BELSORP MAX

Ni-BAND powder/crystal-derived solid · Powder

N2 adsorption measurement used to assess porosity/surface area.

Atmosphere
N2
Context
pristine target framework
Measurement source
4 · Results · Supplementary Fig. 8
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
BET surface area~9 m2/gText
Approximate
4 · Results · Supplementary Fig. 8

Water vapour adsorption gravimetry

Ni-BAND powder/crystal-derived solid · Powder

Sample dried, then exposed to controlled humidity at 298 K; water uptake calculated as (w - w0)/w0.

Temperature
298
Atmosphere
controlled relative humidity
Context
pristine target framework
Measurement source
9 · Methods · Fig. 4b
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
water adsorption at 17% RH0.042846463 g/gSI Table
Exact Reported
# sheet Figure4b · Fig. 4b source data
water adsorption at 70% RH0.061352062 g/gSI Table
Exact Reported
# sheet Figure4b · Fig. 4b source data
water adsorption at 90% RHMarked as a best value within this paper0.123871514 g/gSI Table
Exact Reported
# sheet Figure4b · Fig. 4b source data
water adsorption phase boundariesPhase I <30% RH; Phase II 30-70% RH; Phase III >70% RHText
Qualitative
4 · Results · Fig. 4b