Spectroscopy — In Situ Growth of Lithiophilic MOF Layer Enabling Dendrite-free Lithium Deposition

Measurement evidence

Spectroscopy

In Situ Growth of Lithiophilic MOF Layer Enabling Dendrite-free Lithium Deposition · Yin D., Wang Z., Li Q. et al. · iScience · 2020 · 101869

1 measurement group · 1 results

Reported values remain attached to the sample, method, conditions, extraction quality and source location that produced them.

Raman and FT-IR spectroscopy

Cu-MOF-30 min · Electrode

Cu-MOF-30 min before/after electrolyte immersion and before/after Li cycling.

Geometry
VERTEX 70 for FT-IR; Raman instrument not specified
Context
Cu-MOF-30 min current collector
Measurement source
p004 / journal p.3 · Synthesis and Characterization · Figure S2A-S2C
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
Raman peak shift after electrolyte immersionPeak around 1600 cm^-1 shifts after immersing Cu-MOF-30 min into electrolytearoundText
Approximate
p004 / journal p.3 · Synthesis and Characterization · Figure S2A