TEM, HRTEM and EDX elemental mapping
CuCo-THQ powder · Nanosheet
TEM and HRTEM recorded at 200 kV; EDX mapping used to observe Cu, Co and O distribution.
| Property | Reported value | Normalised value | Uncertainty | Origin and quality | Source |
|---|---|---|---|---|---|
| CuCo-THQ HRTEM d020 spacing | d020 = 11.0 A | — | — | Text Rounded Reported | p004 · 3.1 Synthesis and characterization of photocatalysts · Fig. S5 |
| CuCo-THQ HRTEM d110 spacing | d110 = 11.7 A | — | — | Text Rounded Reported | p004 · 3.1 Synthesis and characterization of photocatalysts · Fig. S5 |