Diffraction Structure — Air-Stability and Carrier Type in Conductive M3(Hexaaminobenzene)2,(M = Co, Ni, Cu)

Measurement evidence

Diffraction Structure

Air-Stability and Carrier Type in Conductive M3(Hexaaminobenzene)2,(M = Co, Ni, Cu) · Hinckley A.C., Park J., Gomes J. et al. · Journal of the American Chemical Society · 2020 · 11123-11130

1 measurement group · 4 results

Reported values remain attached to the sample, method, conditions, extraction quality and source location that produced them.

PXRD with BRUKER D8 Venture and SEM with Magellan 400 XHR

Co-HAB pressed-powder pellet · Pellet

Powder samples before pressing; reproduction confirmed by PXRD and SEM

Context
representative M-HAB pristine MOF powders
Measurement source
S2-S3 · Materials; Instrumentation
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource
Average grain size used in hopping-transport discussionapproximately 2 nm average grain sizeText
Approximate
11124 · Results and Discussion
Cu-HAB synchrotron PXRD cell length signal13.15 AngstromText
Exact Reported
S5 · Computational details
Ni-HAB synchrotron PXRD cell length signal13.11 AngstromText
Exact Reported
S5 · Computational details
M-HAB powder particle sizearound 20-40 nm for all casesrange 20-40 nmText
Range
11124 · Results and Discussion