Linear sweep voltammetry-derived electrical conductivity
Cu-TCNQ powder · Powder
Conductivity sigma determined by LSV; Figure 3e.
| Property | Reported value | Normalised value | Uncertainty | Origin and quality | Source |
|---|---|---|---|---|---|
| Electrical conductivity sigma of pure Cu-TCNQMarked as a best value within this paper | 0.28 S cm^-1 | — | — | Text Exact Reported | 1681 · 3.1 · Figure 3e |