EPR and DC magnetic susceptibility
as-synthesised Ni-TTC black powder · Powder
EPR collected at 90 K; magnetic susceptibility in SQUID-VSM at 1000 Oe
| Property | Reported value | Normalised value | Uncertainty | Origin and quality | Source |
|---|---|---|---|---|---|
| chiM T at 300 K | chiM T = 3.21 emu mol-1 K | — | — | Text Exact Reported | 4 · 2.2. Magnetism of Ni-TTC · Figure 3e |
| Curie constant | 4.35 emu mol-1 K | — | — | Text Exact Reported | 4 · 2.2. Magnetism of Ni-TTC · Figure 3d; Figure S12 |
| EPR g value for high-spin Ni(II) | g = 2.036 | — | — | Text Exact Reported | 4 · 2.1. Synthesis and Structural Characterization of Ni-TTC · Figure 3c |
| Weiss constant | -105.26 K | — | — | Text Exact Reported | 4 · 2.2. Magnetism of Ni-TTC · Figure 3d; Figure S12 |