Thermogravimetric analysis
UiO-66(Zr)-(CO2D)2 characterisation powder · Powder
PerkinElmer STA 6000 under O2, heating rate 2 degC min^-1.
| Property | Reported value | Normalised value | Uncertainty | Origin and quality | Source |
|---|---|---|---|---|---|
| linker degradation onset | higher than 300 degC | — | threshold only | Text Approximate | 2 · Thermogravimetric Analysis (TGA) · Figure S2 |
| oxide formation temperature | above about 770 K | — | about | Text Approximate | 2 · Thermogravimetric Analysis (TGA) · Figure S2 |