Partial recipeSource: Main
Route 1: Other
p006 · Methods - Hydroxide Ion Conductivity Measurement
Metal precursorsas-synthesised NH2-UiO-66 nanoparticles
Linker precursors2-amino-terephthalate framework already formed
Solvents1 mM aqueous KOH
AdditivesKOH hydroxide source
Time24
Work-uppellets equilibrated in constant temperature/humidity environment for 2 h before measurement
Activationpressed into pellets at 20 MPa for 10 s; Ag electrodes evaporated; KOH immersion introduced hydroxide ions
Show 3 structured reagent records
| Role | Reagent | Amount / concentration | Source |
|---|---|---|---|
| Other | as-synthesized NH2-UiO-66 nanoparticles | Not specified | p006 · Methods - Hydroxide Ion Conductivity Measurement |
| Base | KOH aqueous solution | 1 mM | p006 · Methods - Hydroxide Ion Conductivity Measurement |
| Other | silver electrodes | Not specified | p006 · Methods - Hydroxide Ion Conductivity Measurement |