Microscopy Morphology — Biporous Cd(II) Coordination Polymer via in Situ Disulfide Bond Formation: Self-Healing and Application to Photosensitive Optoelectronic Device

Measurement evidence

Microscopy Morphology

Biporous Cd(II) Coordination Polymer via in Situ Disulfide Bond Formation: Self-Healing and Application to Photosensitive Optoelectronic Device · Naskar K., Dey A., Maity S. et al. · Inorganic Chemistry · 2020 · 5518-5528

1 measurement group · 0 results

Reported values remain attached to the sample, method, conditions, extraction quality and source location that produced them.

FESEM imaging, JEOL JSM-6700F

Bulk/crude material of compound 1 · Powder

SEM images before irradiation, after irradiation and after exposure to air.

Atmosphere
air exposure after irradiation
Context
compound 1 crystal before/after reversible photocleavage
Measurement source
5 · Photoreversible Polymerization · Figure S6
PropertyReported valueNormalised valueUncertaintyOrigin and qualitySource