Out-of-plane X-ray diffraction (XRD)
IC-CuTHPP thin-film sensor on ITO interdigital electrode · Electrode
CuTHPP IC-MOF thin films before and after cadaverine detection.
| Property | Reported value | Normalised value | Uncertainty | Origin and quality | Source |
|---|---|---|---|---|---|
| CuTHPP (001) out-of-plane diffraction peak | (001) peak observed at about 12.5 degrees 2theta | — | — | Visual Estimate Approximate | SI p.4 · Supporting Information · Fig. S2 |
| CuTHPP (002) out-of-plane diffraction peak | (002) peak observed at about 26 degrees 2theta | — | — | Visual Estimate Approximate | main p.2, article p.5498 · Results and discussion · Fig. S2 |